工业环氧地坪工程施工如何预防出现裂缝现象

工业环氧地坪工程施工比较容易,是一种主要采用了两次镘涂自流平工艺,平整度大大提高。目前这种产品主要以优质的产品质量,精美的表面设计等赢得了众多客户的赞赏,是目前环氧地坪施工中的领头人,那么我们在平时的生活中如何避免其产品出现裂缝现象,首先:

The construction of industrial epoxy flooring project is relatively easy. It is a kind of self-leveling process which mainly adopts two upsetting coatings, and the smoothness is greatly improved. At present, this product has won the praise of many customers mainly for its high quality product quality and exquisite surface design. It is the leader in the construction of epoxy flooring. So how can we avoid cracks in our daily life? First of all: 1、施工过程把控:

1. The construction process controls:

工业环氧地坪工程施工过程中,首先在材料拌合要选择搅拌机,CV值控制在0.15以内。并且在施工完后保证有2次抹平,这样可以减少裂缝的出现几率。

In the process of construction of industrial epoxy flooring project, first of all, mixer should be selected for material mixing, and CV value should be controlled within 0.15. And after the completion of construction to ensure that there are 2 times to smooth, which can reduce the probability of cracks.

2、混凝土材料质量:

2. The quality of concrete materials:

混凝土主要由水泥、骨料、水、沙石组成,要预防裂缝我们首先要从控制材料开始,水泥我们要尽量选择发热量较低的材料,砂石尽量选用2.4-3.0细度的中砂。

Concrete is mainly composed of cement, aggregate, water and sand. To prevent cracks, we should start with controlling materials. Cement should choose materials with lower calorific value as far as possible, and sand with 2.4-3.0 fineness as possible.

3、基面施工气候:

3. The construction climate of base surface:

混凝土地面出现裂缝,除了材料配比之外,还个主要因素就是气候。因为混凝土地面材料导热性较差,如果温度骤降,会导致表层温度低,内部温度高,导致混凝土因为温差出现裂缝。

In addition to the material ratio, the main factor is the climate. Because the thermal conductivity of concrete surface materials is poor, if the temperature drops sharply, it will lead to low surface temperature and high internal temperature, which will lead to cracks in concrete due to temperature difference.

工业环氧地坪工程基面主要有混凝土地面、砂浆地面、金刚砂耐磨地平面、水磨石地面等,这些地面如果出现裂缝,即便通过砂浆中涂进行修补,裂缝依旧会在日后慢慢扩展延伸,加宽加长,并且会直接作用于工业环氧地坪工程涂料层,导致工业环氧地坪工程出现裂缝。

Industrial epoxy floor engineering base surface mainly includes concrete floor, mortar floor, diamond wear-resistant floor, terrazzo floor and so on. If these ground surface cracks occur, even if repaired through mortar coating, the cracks will continue to expand and extend slowly in the future, widen and lengthen, and will directly affect the industrial floor engineering coating. The material layer leads to cracks in the industrial floor project.


辛苦整理 请保留:http://www.rfl5.com/shownews.asp?id=1603

版权所有:常州市三顾环保设备有限公司主营:热风炉/燃油热风炉/燃煤热风炉/燃气热风炉/生物质热风炉 地 址:江苏省常州市武进区洛阳镇   手 机:13921030623 顾培建
电 话:0519-83756711    传 真:0519-83756711  邮 箱:cz3_gu@126.com  网址:http://www.rfl5.ccom    苏ICP备12038950号   网站地图